  <dc:creator>Guerrero-Alburquerque, Natalia</dc:creator>
  <dc:creator>Zhao, Shanyu</dc:creator>
  <dc:creator>Adilien, Nour</dc:creator>
  <dc:creator>Koebel, Matthias M.</dc:creator>
  <dc:creator>Lattuada, Marco</dc:creator>
  <dc:creator>Malfait, Wim J.</dc:creator>
  <dc:date>2020-05-13</dc:date>
  <dc:description xmlns:ns0="xml" ns0:lang="en">Biopolymer aerogels are an emerging class of materials with potential applications in  drug delivery, thermal insulation, separation, and filtration. Chitosan is of particular  interest as a sustainable, biocompatible, and abundant raw material. Here, we present  urea-modified chitosan aerogels with a high surface area and excellent thermal and  mechanical properties. The irreversible gelation of an acidic chitosan solution is  triggered by the thermal decomposition of urea at 80 °C through an increase in pH  and, more importantly, the formation of abundant ureido terminal groups. The  hydrogels are dried using either supercritical CO2 drying (SCD) or ambient pressure  drying (APD) methods to elucidate the influence of the drying process on the final  aerogel properties. The hydrogels are exchanged into ethanol prior to SCD, and into  ethanol and then heptane prior to APD. The surface chemistry and microstructure are  monitored by solid-state NMR and Fourier transform infrared spectroscopy, scanning  electron microscopy, and nitrogen sorption. Surprisingly, large monolithic aerogel  plates (70 × 70 mm2) can be produced by APD, albeit at a somewhat higher density  (0.17–0.42 g/cm3). The as prepared aerogels have thermal conductivities of ∼24 and  ∼31 mW/(m·K) and surface areas of 160–170 and 85–230 m2/g, for SCD and APD,  respectively. For a primarily biopolymer-based material, these aerogels are  exceptionally stable at elevated temperature (TGA) and char and self-extinguish after  direct flame exposure. The urea-modified chitosan aerogels display superior  mechanical properties compared to traditional silica aerogels, with no brittle rupture up  to at least 80% strain, and depending on the chitosan concentration, relatively high E- moduli (1.0–11.6 MPa), and stress at 80% strain values (σ80 of 3.5–17.9 MPa).  Remarkably, the aerogel monoliths can be shaped and machined with standard tools,  for example, drilling and sawing. This first demonstration to produce monolithic and  machinable, mesoporous aerogels from bio-sourced, renewable, and nontoxic  precursors, combined with the potential for reduced production cost by means of  simple APD, opens up new opportunities for biopolymer aerogel applications and  marks an important step toward commercialization of biopolymer aerogels.</dc:description>
  <dc:format>application/pdf</dc:format>
  <dc:identifier>https://folia.unifr.ch/unifr/documents/308724</dc:identifier>
  <dc:identifier>https://folia.unifr.ch/documents/308724/files/lat_smi.pdf</dc:identifier>
  <dc:identifier>https://folia.unifr.ch/documents/308724/files/lat_smi_sm1.pdf</dc:identifier>
  <dc:identifier>https://folia.unifr.ch/documents/308724/files/lat_smi_sm2.txt</dc:identifier>
  <dc:language>eng</dc:language>
  <dc:relation>info:eu-repo/semantics/altIdentifier/doi/10.1021/acsami.0c03047</dc:relation>
  <dc:rights>info:eu-repo/semantics/openAccess</dc:rights>
  <dc:rights>License undefined</dc:rights>
  <dc:source>ACS Applied Materials &amp; Interfaces. - 2020, vol. 12, no. 19, p. 22037–22049</dc:source>
  <dc:subject>info:eu-repo/classification/udc/54</dc:subject>
  <dc:title xmlns:ns1="xml" ns1:lang="en">Strong, machinable, and insulating chitosan–urea aerogels: toward ambient pressure drying of biopolymer aerogel monoliths</dc:title>